PLA settings for the Anycubic Kobra S1
Last updated 9 November 2026
OrcaSlicer's Anycubic PLA profile prints at 205 °C, with the bed at 55 °C and the part fan at 100 %.
| Profile | Nozzle | Bed | Part fan | Max flow | Retraction |
|---|---|---|---|---|---|
| Anycubic PLA | 205 °C | 55 °C | 100 % | 12 mm³/s | 0.8 mm |
| Anycubic PLA High Speed | 205 °C | 55 °C | 100 % | 18 mm³/s | 0.8 mm |
| Anycubic PLA Silk | 230 °C | 55 °C | 100 % | 12 mm³/s | 0.8 mm |
| Anycubic PLA+ | 210 °C | 55 °C | 100 % | 15 mm³/s | 0.8 mm |
| Panchroma PLA | 220 °C | 50 °C | 100 % | 20 mm³/s | 0.8 mm |
| Polymaker PLA Pro | 220 °C | 50 °C | 100 % | 16 mm³/s | 0.8 mm |
| Polymaker PLA Pro Metallic | 220 °C | 50 °C | 100 % | 16 mm³/s | 0.8 mm |
| AliZ PLA | 220 °C | 55 °C | 100 % | 12 mm³/s | 0.8 mm |
| OrcaSlicer has 140 more PLA profiles for this printer. |
How do I set up my file for the Anycubic Kobra S1?
Drop it here. It opens in Convert with the Anycubic Kobra S1 and Anycubic PLA picked, and nothing converts until you click Convert.
Which build plate should I use?
Anycubic PLA sets a bed temperature for each plate:
- Textured PEI plate: 55 °C
- Smooth PEI plate: 55 °C
- Cool plate: 35 °C
- Engineering plate: not supported
Why won't my PLA stick?
Anycubic PLA heats the bed to 55 °C, so wipe the sheet with 90 % or stronger isopropyl alcohol before you print (Prusa Knowledge Base). If a corner still lifts, add a brim (Prusa Knowledge Base).
Why is my PLA stringing?
Try 5 to 10 °C below the 205 °C that Anycubic PLA sets, since a cooler nozzle strings less (Prusa Knowledge Base). A spool that has taken on moisture strings badly, so try a dry one (Prusa Knowledge Base).
Why does PLA clog in an enclosed printer?
Anycubic PLA heats the bed to 55 °C, and PLA softens below 60 °C, so open the door or lid once the bed passes 45 °C (Bambu Lab wiki).
Where do these values come from?
From the profiles OrcaSlicer ships, read at OrcaSlicer v2.4.2 (8500fcd). Where a filament profile leaves retraction unset, the table shows the printer profile's value.