PETG settings for the Creality Ender-3 V3 KE
Last updated 9 November 2026
Creality Print's CR-PETG profile prints at 230 °C, with the bed at 70 °C and the part fan at 30 to 40 %.
| Profile | Nozzle | Bed | Part fan | Max flow | Retraction |
|---|---|---|---|---|---|
| CR-PETG | 230 °C | 70 °C | 30 to 40 % | 9 mm³/s | 0.8 mm |
| Soleyin Basic PETG | 240 °C | 70 °C | 40 to 80 % | 9 mm³/s | 0.8 mm |
How do I set up my file for the Creality Ender-3 V3 KE?
Drop it here. It opens in Convert with the Creality Ender-3 V3 KE and CR-PETG picked, and nothing converts until you click Convert.
Which build plate should I use?
CR-PETG sets a bed temperature for each plate:
- Textured PEI plate: 70 °C
- Smooth PEI plate: 70 °C
- Cool plate: 70 °C
- Engineering plate: not supported
Why is my PETG stringing?
Wet PETG strings more, so dry it at 60 to 65 °C for 8 hours (Bambu Lab wiki). If the spool is dry, try 5 to 10 °C below the 230 °C that CR-PETG sets, but not below its 220 °C floor (Prusa Knowledge Base). Keep the part fan on, since cooling PETG prevents stringing, and lengthen retraction (Prusa Knowledge Base).
Why does PETG print so slowly?
CR-PETG caps flow at 9 mm³/s, and the slicer slows any move that would push more plastic than that (slicer source).
Why does my PETG lift or warp?
CR-PETG heats the bed to 70 °C, so clean the sheet first, then add a brim (Prusa Knowledge Base). On smooth PEI, apply a glue stick first, since PETG can bond hard enough to damage the sheet (Prusa Knowledge Base).
Where do these values come from?
From the profiles Creality Print ships, read at CrealityPrint v7.3.1 (254250c). Where a filament profile leaves retraction unset, the table shows the printer profile's value.