TPU settings for the Creality Ender-3 in Cura
Last updated 9 November 2026
Cura's Velleman TPU profile prints at 220 °C, with the bed at 0 °C and the part fan at 20 %.
| Profile | Nozzle | Bed | Part fan | Max flow | Retraction |
|---|---|---|---|---|---|
| Velleman TPU | 220 °C | 0 °C | 20 % | not declared | 3 mm |
| eMotionTech TPU | 235 °C | 60 °C | 100 % | not declared | 1.3 mm |
| Eryone TPU | 235 °C | 50 °C | 100 % | not declared | 6 mm |
| FABtotum TPU | 220 °C | 40 °C | 100 % | not declared | 6.5 mm |
| GOOFOO TPU | 210 °C | 60 °C | 100 % | not declared | 1 mm |
| GOOFOO TPU | 220 °C | 50 °C | 100 % | not declared | 1 mm |
| Volumic TPU | 235 °C | 45 °C | 75 % | not declared | 3 mm |
| XYZprinting TPU | 210 °C | 45 °C | 100 % | not declared | 6.5 mm |
| Cura has 1 more TPU profiles for this printer. |
How do I set up my file for the Creality Ender-3?
Drop it here. It opens in Convert with the Creality Ender-3 and Velleman TPU picked, and nothing converts until you click Convert.
Why won't my TPU feed?
Feed TPU from a spool that turns freely, since drag on the soft filament starves the nozzle (Bambu Lab wiki). Run it through a multi-spool feeder only if the spool is sold for one (Bambu Lab wiki). Print slowly, about 20 mm/s, since a fast feed can tangle TPU in the extruder gears (Prusa Knowledge Base).
Why is my TPU stringing?
Wet TPU strings, so dry the spool first (Bambu Lab wiki). Print the parts one at a time rather than layer by layer, so the nozzle travels less between them (Bambu Lab wiki). If it still strings, lengthen retraction 0.2 mm at a time from the 3 mm that Velleman TPU sets (Bambu Lab wiki).
Do I need to dry TPU?
Yes, dry TPU at 70 °C for 8 hours before printing (Bambu Lab wiki). TPU takes on moisture fast, so store it sealed with desiccant between prints (Bambu Lab wiki).
Where do these values come from?
From the profiles Cura ships, read at Cura main (42dbd93). Where a filament profile leaves retraction unset, the table shows the printer profile's value.