TPU settings for the Creality Hi

Last updated 9 November 2026

Creality Print's HP-TPU profile prints at 220 °C, with the bed at 40 °C and the part fan at 100 %.

Profile Nozzle Bed Part fan Max flow Retraction
HP-TPU 220 °C 40 °C 100 % 3 mm³/s 2 mm

How do I set up my file for the Creality Hi?

Drop it here. It opens in Convert with the Creality Hi and HP-TPU picked, and nothing converts until you click Convert.

Which build plate should I use?

HP-TPU sets a bed temperature for each plate:

  • Textured PEI plate: 40 °C
  • Smooth PEI plate: 40 °C
  • Cool plate: 40 °C
  • Engineering plate: 35 °C

Why won't my TPU feed?

Feed TPU from a spool that turns freely, since drag on the soft filament starves the nozzle (Bambu Lab wiki). Run it through a multi-spool feeder only if the spool is sold for one (Bambu Lab wiki). Print slowly, about 20 mm/s, since a fast feed can tangle TPU in the extruder gears (Prusa Knowledge Base).

Why is my TPU stringing?

Wet TPU strings, so dry the spool first (Bambu Lab wiki). Print the parts one at a time rather than layer by layer, so the nozzle travels less between them (Bambu Lab wiki). If it still strings, lengthen retraction 0.2 mm at a time from the 2 mm that HP-TPU sets (Bambu Lab wiki).

Do I need to dry TPU?

Yes, dry TPU at 70 °C for 8 hours before printing (Bambu Lab wiki). TPU takes on moisture fast, so store it sealed with desiccant between prints (Bambu Lab wiki).

Where do these values come from?

From the profiles Creality Print ships, read at CrealityPrint v7.3.1 (254250c). Where a filament profile leaves retraction unset, the table shows the printer profile's value.

Something wrong or missing on this page? feedback@lovlar.dev

Slicer and printer names belong to their owners. preslice is not affiliated with them.