TPU settings for the Flashforge Adventurer 5M

Last updated 9 November 2026

OrcaSlicer's Flashforge Generic TPU profile prints at 225 °C, with the bed at 45 °C and the part fan at 100 %.

Profile Nozzle Bed Part fan Max flow Retraction
Flashforge Generic TPU 225 °C 45 °C 100 % 3.5 mm³/s 1.2 mm
Flashforge TPU 95A 225 °C 45 °C 100 % 3.5 mm³/s 1.2 mm
Bambu TPU 95A 230 °C 35 °C 100 % 3.6 mm³/s 0.4 mm
Bambu TPU 95A HF 230 °C 35 °C 100 % 12 mm³/s 0.8 mm
COEX TPE 30D 240 °C 35 °C 80 to 100 % 3.5 mm³/s 0.4 mm
COEX TPE 40D 240 °C 35 °C 80 to 100 % 5.5 mm³/s 0.4 mm
COEX TPE 60D 240 °C 35 °C 80 to 100 % 6.5 mm³/s 0.4 mm
COEX TPU 60A 225 °C 35 °C 80 to 100 % 1 mm³/s 0 mm
OrcaSlicer has 9 more TPU profiles for this printer.

How do I set up my file for the Flashforge Adventurer 5M?

Drop it here. It opens in Convert with the Flashforge Adventurer 5M and Flashforge Generic TPU picked, and nothing converts until you click Convert.

Which build plate should I use?

Flashforge Generic TPU sets a bed temperature for each plate:

  • Textured PEI plate: 60 °C
  • Smooth PEI plate: 45 °C
  • Cool plate: 60 °C
  • Engineering plate: 60 °C

Why won't my TPU feed?

Feed TPU from a spool that turns freely, since drag on the soft filament starves the nozzle (Bambu Lab wiki). Run it through a multi-spool feeder only if the spool is sold for one (Bambu Lab wiki). Print slowly, about 20 mm/s, since a fast feed can tangle TPU in the extruder gears (Prusa Knowledge Base).

Why is my TPU stringing?

Wet TPU strings, so dry the spool first (Bambu Lab wiki). Print the parts one at a time rather than layer by layer, so the nozzle travels less between them (Bambu Lab wiki). If it still strings, lengthen retraction 0.2 mm at a time from the 1.2 mm that Flashforge Generic TPU sets (Bambu Lab wiki).

Do I need to dry TPU?

Yes, dry TPU at 70 °C for 8 hours before printing (Bambu Lab wiki). TPU takes on moisture fast, so store it sealed with desiccant between prints (Bambu Lab wiki).

Where do these values come from?

From the profiles OrcaSlicer ships, read at OrcaSlicer v2.4.2 (8500fcd). Where a filament profile leaves retraction unset, the table shows the printer profile's value.

Something wrong or missing on this page? feedback@lovlar.dev