Last updated 9 November 2026
PrusaSlicer's Prusament PLA profile prints at 215 °C, with the bed at 60 °C and the part fan at 100 %.
| Profile | Nozzle | Bed | Part fan | Max flow | Retraction |
|---|---|---|---|---|---|
| Prusament PLA | 215 °C | 60 °C | 100 % | 15 mm³/s | 3.2 mm |
| 3D-Fuel Standard PLA+ | 220 °C | 60 °C | 100 % | 10 mm³/s | 3.2 mm |
| 3D-Fuel Tough PLA+ | 230 °C | 60 °C | 100 % | 10 mm³/s | 3.2 mm |
| Alzament Basic PLA | 215 °C | 60 °C | 100 % | 15 mm³/s | 3.2 mm |
| AmazonBasics PLA | 210 °C | 60 °C | 100 % | 15 mm³/s | 3.2 mm |
| Buddy3D PLA | 215 °C | 60 °C | 100 % | 15 mm³/s | 3.2 mm |
| ColorFabb PLA-PHA | 210 °C | 60 °C | 100 % | 10 mm³/s | 3.2 mm |
| ColorFabb bronzeFill | 210 °C | 60 °C | 100 % | 4 mm³/s | 3.2 mm |
| PrusaSlicer has 137 more PLA profiles for this printer. |
How do I set up my file for the Original Prusa MINI?
Drop it here. It opens in Convert with the Original Prusa MINI and Prusament PLA picked, and nothing converts until you click Convert.
Why won't my PLA stick?
Prusament PLA heats the bed to 60 °C, so wipe the sheet with 90 % or stronger isopropyl alcohol before you print (Prusa Knowledge Base). If a corner still lifts, add a brim (Prusa Knowledge Base).
Why is my PLA stringing?
Try 5 to 10 °C below the 215 °C that Prusament PLA sets, since a cooler nozzle strings less (Prusa Knowledge Base). A spool that has taken on moisture strings badly, so try a dry one (Prusa Knowledge Base).
Where do these values come from?
From the profiles PrusaSlicer ships, read at PrusaSlicer 2.9.6 profiles (3f2935e). Where a filament profile leaves retraction unset, the table shows the printer profile's value.