PLA settings for the Sovol SV08

Last updated 9 November 2026

OrcaSlicer's Sovol SV08 PLA profile prints at 220 °C, with the bed at 65 °C and the part fan at 50 to 70 %.

Profile Nozzle Bed Part fan Max flow Retraction
Sovol SV08 PLA 220 °C 65 °C 50 to 70 % 21 mm³/s 0.5 mm
AliZ PLA 220 °C 55 °C 100 % 12 mm³/s 0.5 mm
Bambu PLA Basic 220 °C 55 °C 100 % 21 mm³/s 0.5 mm
Bambu PLA Dynamic 220 °C 55 °C 100 % 21 mm³/s 0.5 mm
Bambu PLA Galaxy 220 °C 55 °C 100 % 12 mm³/s 0.5 mm
Bambu PLA Glow 220 °C 55 °C 100 % 12 mm³/s 0.5 mm
Bambu PLA Impact 220 °C 55 °C 100 % 23.2 mm³/s 0.5 mm
Bambu PLA Marble 220 °C 55 °C 100 % 12 mm³/s 0.5 mm
OrcaSlicer has 134 more PLA profiles for this printer.

How do I set up my file for the Sovol SV08?

Drop it here. It opens in Convert with the Sovol SV08 and Sovol SV08 PLA picked, and nothing converts until you click Convert.

Which build plate should I use?

Sovol SV08 PLA sets a bed temperature for each plate:

  • Textured PEI plate: 55 °C
  • Smooth PEI plate: 65 °C
  • Cool plate: 35 °C
  • Engineering plate: not supported
  • SuperTack plate: 45 °C

Why won't my PLA stick?

Sovol SV08 PLA heats the bed to 65 °C, so wipe the sheet with 90 % or stronger isopropyl alcohol before you print (Prusa Knowledge Base). If a corner still lifts, add a brim (Prusa Knowledge Base).

Why is my PLA stringing?

Try 5 to 10 °C below the 220 °C that Sovol SV08 PLA sets, since a cooler nozzle strings less (Prusa Knowledge Base). A spool that has taken on moisture strings badly, so try a dry one (Prusa Knowledge Base).

Where do these values come from?

From the profiles OrcaSlicer ships, read at OrcaSlicer v2.4.2 (8500fcd). Where a filament profile leaves retraction unset, the table shows the printer profile's value.