PLA settings for the Anycubic Kobra 2 Neo

OrcaSlicer's Anycubic PLA profile prints at 190 °C, with the bed at 60 °C and the part fan at 80 to 100 %.

Profile Nozzle Bed Part fan Max flow Retraction
Anycubic PLA 190 °C 60 °C 80 to 100 % 12 mm³/s 2.5 mm
AliZ PLA 220 °C 55 °C 100 % 12 mm³/s 2.5 mm
Bambu PLA Basic 220 °C 55 °C 100 % 21 mm³/s 2.5 mm
Bambu PLA Dynamic 220 °C 55 °C 100 % 21 mm³/s 2.5 mm
Bambu PLA Galaxy 220 °C 55 °C 100 % 12 mm³/s 2.5 mm
Bambu PLA Glow 220 °C 55 °C 100 % 12 mm³/s 2.5 mm
Bambu PLA Impact 220 °C 55 °C 100 % 23.2 mm³/s 2.5 mm
Bambu PLA Marble 220 °C 55 °C 100 % 12 mm³/s 2.5 mm
OrcaSlicer has 134 more PLA profiles for this printer.

How do I set up my file for the Anycubic Kobra 2 Neo?

Drop it here. It opens in Convert with the Anycubic Kobra 2 Neo and Anycubic PLA picked, and nothing converts until you click Convert.

Which build plate should I use?

Anycubic PLA sets a bed temperature for each plate:

  • Textured PEI plate: 45 °C
  • Smooth PEI plate: 60 °C
  • Cool plate: 35 °C
  • Engineering plate: not supported

Why is my PLA stringing?

Try 5 to 10 °C below the 190 °C that Anycubic PLA sets, since a cooler nozzle strings less (Prusa Knowledge Base). A spool that has taken on moisture strings badly, so try a dry one (Prusa Knowledge Base).

Where do these values come from?

From the profiles OrcaSlicer ships, read at OrcaSlicer v2.4.2 (8500fcd). Where a filament profile leaves retraction unset, the table shows the printer profile's value.