PLA settings for the Anycubic Kobra 3
OrcaSlicer's Anycubic PLA profile prints at 210 °C, with the bed at 60 °C and the part fan at 60 to 80 %.
| Profile | Nozzle | Bed | Part fan | Max flow | Retraction |
|---|---|---|---|---|---|
| Anycubic PLA | 210 °C | 60 °C | 60 to 80 % | 12 mm³/s | 1 mm |
| Anycubic Generic PLA | 220 °C | 45 °C | 100 % | 12 mm³/s | 1 mm |
| Anycubic PLA Glow | 210 °C | 60 °C | 80 to 100 % | 7.2 mm³/s | 0.8 mm |
| Anycubic PLA High Speed | 210 °C | 65 °C | 80 to 100 % | 18 mm³/s | 2.5 mm |
| Anycubic PLA Matte | 210 °C | 65 °C | 80 to 100 % | 9 mm³/s | 0.8 mm |
| Anycubic PLA SE | 210 °C | 65 °C | 80 to 100 % | 12 mm³/s | 0.8 mm |
| Anycubic PLA Slik | 220 °C | 65 °C | 80 to 100 % | 7.2 mm³/s | 0.5 mm |
| Anycubic PLA+ | 230 °C | 65 °C | 80 to 100 % | 12 mm³/s | 1 mm |
| OrcaSlicer has 141 more PLA profiles for this printer. |
How do I set up my file for the Anycubic Kobra 3?
Drop it here. It opens in Convert with the Anycubic Kobra 3 and Anycubic PLA picked, and nothing converts until you click Convert.
Which build plate should I use?
Anycubic PLA sets a bed temperature for each plate:
- Textured PEI plate: 45 °C
- Smooth PEI plate: 60 °C
- Cool plate: 35 °C
- Engineering plate: not supported
Why is my PLA stringing?
Try 5 to 10 °C below the 210 °C that Anycubic PLA sets, since a cooler nozzle strings less (Prusa Knowledge Base). A spool that has taken on moisture strings badly, so try a dry one (Prusa Knowledge Base).
Where do these values come from?
From the profiles OrcaSlicer ships, read at OrcaSlicer v2.4.2 (8500fcd). Where a filament profile leaves retraction unset, the table shows the printer profile's value.