PLA settings for the Creality Ender-3 V3 SE
Creality Print's Hyper PLA profile prints at 190 °C, with the bed at 50 °C and the part fan at 100 %.
| Profile | Nozzle | Bed | Part fan | Max flow | Retraction |
|---|---|---|---|---|---|
| Hyper PLA | 190 °C | 50 °C | 100 % | 23 mm³/s | 1.2 mm |
| CR-PLA | 190 °C | 50 °C | 100 % | 12 mm³/s | 1 mm |
| Hyper L-W PLA | 220 °C | 60 °C | 60 to 100 % | 4 mm³/s | 0.6 mm |
| Hyper Luminous | 220 °C | 50 °C | 100 % | 16 mm³/s | 0.8 mm |
| Hyper Marble | 220 °C | 50 °C | 100 % | 18 mm³/s | 1.5 mm |
| Hyper Stardust | 220 °C | 50 °C | 100 % | 18 mm³/s | 2 mm |
| Soleyin Ultra PLA | 220 °C | 50 °C | 100 % | 16 mm³/s | 0.8 mm |
How do I set up my file for the Creality Ender-3 V3 SE?
Drop it here. It opens in Convert with the Creality Ender-3 V3 SE and Hyper PLA picked, and nothing converts until you click Convert.
Which build plate should I use?
Hyper PLA sets a bed temperature for each plate:
- Textured PEI plate: 50 °C
- Smooth PEI plate: 50 °C
- Cool plate: 50 °C
- Engineering plate: 45 °C
Why is my PLA stringing?
Try 5 to 10 °C below the 190 °C that Hyper PLA sets, since a cooler nozzle strings less (Prusa Knowledge Base). A spool that has taken on moisture strings badly, so try a dry one (Prusa Knowledge Base).
Where do these values come from?
From the profiles Creality Print ships, read at CrealityPrint v7.3.1 (254250c). Where a filament profile leaves retraction unset, the table shows the printer profile's value.