PLA settings for the Elegoo Centauri Carbon 2

OrcaSlicer's Elegoo PLA profile prints at 210 °C, with the bed at 60 °C and the part fan at 50 to 100 %.

Profile Nozzle Bed Part fan Max flow Retraction
Elegoo PLA 210 °C 60 °C 50 to 100 % 21 mm³/s 0.8 mm
Elegoo PLA Basic 220 °C 60 °C 50 to 100 % 21 mm³/s 0.8 mm
Elegoo PLA Galaxy 220 °C 60 °C 80 to 100 % 18 mm³/s 0.8 mm
Elegoo PLA Glow 220 °C 60 °C 100 % 18 mm³/s 0.8 mm
Elegoo PLA Marble 220 °C 60 °C 80 to 100 % 18 mm³/s 0.8 mm
Elegoo PLA Matte 220 °C 60 °C 60 to 80 % 16 mm³/s 0.8 mm
Elegoo PLA PRO 220 °C 60 °C 50 to 100 % 20 mm³/s 0.8 mm
Elegoo PLA Silk 230 °C 60 °C 60 to 80 % 16 mm³/s 0.8 mm
OrcaSlicer has 148 more PLA profiles for this printer.

How do I set up my file for the Elegoo Centauri Carbon 2?

Drop it here. It opens in Convert with the Elegoo Centauri Carbon 2 and Elegoo PLA picked, and nothing converts until you click Convert.

Which build plate should I use?

Elegoo PLA sets a bed temperature for each plate:

  • Textured PEI plate: 60 °C
  • Smooth PEI plate: 60 °C
  • Cool plate: 35 °C
  • Engineering plate: not supported

Why is my PLA stringing?

Try 5 to 10 °C below the 210 °C that Elegoo PLA sets, since a cooler nozzle strings less (Prusa Knowledge Base). A spool that has taken on moisture strings badly, so try a dry one (Prusa Knowledge Base).

Why does PLA clog in an enclosed printer?

Elegoo PLA heats the bed to 60 °C, and PLA softens below 60 °C, so Bambu Lab says to open the front door or remove the top glass once the bed passes 45 °C (Bambu Lab wiki).

Where do these values come from?

From the profiles OrcaSlicer ships, read at OrcaSlicer v2.4.2 (8500fcd). Where a filament profile leaves retraction unset, the table shows the printer profile's value.