PETG settings for the Elegoo Neptune 4 Max

OrcaSlicer's Generic PETG profile prints at 240 °C, with the bed at 80 °C and the part fan at 20 to 50 %.

Profile Nozzle Bed Part fan Max flow Retraction
Generic PETG 240 °C 80 °C 20 to 50 % 10 mm³/s 0.8 mm
Elegoo PETG 250 °C 70 °C 10 to 40 % 11 mm³/s 0.8 mm
Elegoo PETG PRO 240 °C 70 °C 10 to 40 % 8 mm³/s 0.8 mm
Elegoo PETG Translucent 255 °C 70 °C 10 to 35 % 10 mm³/s 0.8 mm
Elegoo PETG-CF 250 °C 70 °C 5 to 40 % 15 mm³/s 0.8 mm
Elegoo PETG-GF 250 °C 70 °C 5 to 40 % 12 mm³/s 0.8 mm
Elegoo Rapid PETG 250 °C 70 °C 30 to 80 % 18 mm³/s 0.8 mm
Generic PETG PRO 240 °C 70 °C 10 to 40 % 8 mm³/s 0.8 mm
OrcaSlicer has 42 more PETG profiles for this printer.

How do I set up my file for the Elegoo Neptune 4 Max?

Drop it here. It opens in Convert with the Elegoo Neptune 4 Max and Generic PETG picked, and nothing converts until you click Convert.

Which build plate should I use?

Generic PETG sets a bed temperature for each plate:

  • Textured PEI plate: 80 °C
  • Smooth PEI plate: 80 °C
  • Cool plate: 60 °C
  • Engineering plate: not supported

Why is my PETG stringing?

Lower the nozzle toward 220 °C, the floor Generic PETG declares, and lengthen retraction (Prusa Knowledge Base). Wet PETG strings more, and Bambu Lab dries it at 60 to 65 °C for 8 hours in a forced-air oven (Bambu Lab wiki).

Why does PETG print so slowly?

Generic PETG caps flow at 10 mm³/s, and the slicer slows any move that would push more plastic than that (slicer source).

Why won't my PETG stick?

Generic PETG heats the bed to 80 °C, so if a part still lifts, clean the sheet first (Prusa Knowledge Base). On smooth PEI, apply a glue stick first, since PETG can bond hard enough to damage the sheet (Prusa Knowledge Base).

Where do these values come from?

From the profiles OrcaSlicer ships, read at OrcaSlicer v2.4.2 (8500fcd). Where a filament profile leaves retraction unset, the table shows the printer profile's value.