PLA settings for the Flashforge Adventurer 5M
OrcaSlicer's Flashforge Generic PLA profile prints at 220 °C, with the bed at 50 °C and the part fan at 100 %.
| Profile | Nozzle | Bed | Part fan | Max flow | Retraction |
|---|---|---|---|---|---|
| Flashforge Generic PLA | 220 °C | 50 °C | 100 % | 25 mm³/s | 0.8 mm |
| Flashforge Generic HS PLA | 220 °C | 50 °C | 100 % | 25 mm³/s | 0.8 mm |
| Flashforge Generic PLA-Silk | 220 °C | 50 °C | 100 % | 12 mm³/s | 0.8 mm |
| Flashforge HS PLA | 220 °C | 50 °C | 100 % | 25 mm³/s | 0.8 mm |
| Flashforge PLA Basic | 220 °C | 50 °C | 100 % | 25 mm³/s | 0.8 mm |
| Flashforge PLA Color Change | 220 °C | 50 °C | 100 % | 25 mm³/s | 0.8 mm |
| Flashforge PLA Galaxy | 220 °C | 50 °C | 100 % | 25 mm³/s | 0.8 mm |
| Flashforge PLA Luminous | 220 °C | 50 °C | 100 % | 25 mm³/s | 0.8 mm |
| OrcaSlicer has 152 more PLA profiles for this printer. |
How do I set up my file for the Flashforge Adventurer 5M?
Drop it here. It opens in Convert with the Flashforge Adventurer 5M and Flashforge Generic PLA picked, and nothing converts until you click Convert.
Which build plate should I use?
Flashforge Generic PLA sets a bed temperature for each plate:
- Textured PEI plate: 60 °C
- Smooth PEI plate: 50 °C
- Cool plate: 60 °C
- Engineering plate: 60 °C
Why is my PLA stringing?
Try 5 to 10 °C below the 220 °C that Flashforge Generic PLA sets, since a cooler nozzle strings less (Prusa Knowledge Base). A spool that has taken on moisture strings badly, so try a dry one (Prusa Knowledge Base).
Where do these values come from?
From the profiles OrcaSlicer ships, read at OrcaSlicer v2.4.2 (8500fcd). Where a filament profile leaves retraction unset, the table shows the printer profile's value.