PLA settings for the Voron 2.4 350
OrcaSlicer's Generic PLA profile prints at 220 °C, with the bed at 55 °C and the part fan at 100 %.
| Profile | Nozzle | Bed | Part fan | Max flow | Retraction |
|---|---|---|---|---|---|
| Generic PLA | 220 °C | 55 °C | 100 % | 12 mm³/s | 0.8 mm |
| AliZ PLA | 220 °C | 55 °C | 100 % | 12 mm³/s | 0.8 mm |
| Bambu PLA Basic | 220 °C | 55 °C | 100 % | 21 mm³/s | 0.8 mm |
| Bambu PLA Dynamic | 220 °C | 55 °C | 100 % | 21 mm³/s | 0.8 mm |
| Bambu PLA Galaxy | 220 °C | 55 °C | 100 % | 12 mm³/s | 0.8 mm |
| Bambu PLA Glow | 220 °C | 55 °C | 100 % | 12 mm³/s | 0.8 mm |
| Bambu PLA Impact | 220 °C | 55 °C | 100 % | 23.2 mm³/s | 0.8 mm |
| Bambu PLA Marble | 220 °C | 55 °C | 100 % | 12 mm³/s | 0.8 mm |
| OrcaSlicer has 133 more PLA profiles for this printer. |
How do I set up my file for the Voron 2.4 350?
Drop it here. It opens in Convert with the Voron 2.4 350 and Generic PLA picked, and nothing converts until you click Convert.
Which build plate should I use?
Generic PLA sets a bed temperature for each plate:
- Textured PEI plate: 55 °C
- Smooth PEI plate: 55 °C
- Cool plate: 35 °C
- Engineering plate: not supported
- SuperTack plate: 45 °C
Why is my PLA stringing?
Try 5 to 10 °C below the 220 °C that Generic PLA sets, since a cooler nozzle strings less (Prusa Knowledge Base). A spool that has taken on moisture strings badly, so try a dry one (Prusa Knowledge Base).
Why does PLA clog in an enclosed printer?
Generic PLA heats the bed to 55 °C, and PLA softens below 60 °C, so Bambu Lab says to open the front door or remove the top glass once the bed passes 45 °C (Bambu Lab wiki).
Where do these values come from?
From the profiles OrcaSlicer ships, read at OrcaSlicer v2.4.2 (8500fcd). Where a filament profile leaves retraction unset, the table shows the printer profile's value.